Roditi   About Contacts Stock Email Home

Neodymium Doped Yttrium Lithium Fluoride
Nd:YLF

Nd_YAGOur Nd:YLF crystals are grown using the Czochralski technique. The use of high quality starting materials for crystal growth, whole boule interferometry, and precise measurement of bulk losses using transmission spectroscopy assures that each crystal will perform to customer specifications. Each rod is laser inspected to ensure that they free from bubbles and inclusions. Full traceability on all material produced, from finished laser material back to starting chemicals, is maintained.

The Nd:YLF material Roditi is able to supply includes:


Typical finished part specifications are listed below:

Specifications:

Standard Dopant: 1.1±0.1%
Parallelism: <10 arc seconds
Perpendicularity: <5 arc minutes
Chamfer: 0.1mm@45º
Surface Quality: 10/5
Surface Flatness: λ/10 @ 632.8nm
End Coating: R<0.15% @ 1047/1053nm
Laser Damage Threshold 15 J/cm2, 10ns, 10Hz

To discuss your requirements further please call us or email sales@roditi.com

Specification subject to change without notice. Roditi International 2007